Özet
The renovation and widening project for Golden Horn Bridge on the way of first Boshporus Bridge connecting Asia to Europa s an interesting event because it is a steel-concrete complex structure and shows the developments in welded bridge structions by years. In this paper this project is given and the welding procedure tests are studied from both weld plans and applicable welding procedure specifications.
| Orijinal dil | İngilizce |
|---|---|
| Sayfa (başlangıç-bitiş) | 141-159 |
| Sayfa sayısı | 19 |
| Dergi | Welding in the World, Le Soudage Dans Le Monde |
| Hacim | 38 |
| Yayın durumu | Yayınlandı - Kas 1996 |
| Etkinlik | Proceedings of the 1996 International Conference on Welded Structures, in Particular Welded Bridges - Budapest, Hung Süre: 2 Eyl 1996 → 3 Eyl 1996 |