Trend surface analysis of primary rock samples from a region of copper and zinc mineralization; Maden Complex, SE-Turkey

  • Istanbul Technical University

Araştırma çıktısı: Dergi yayınıMakaleHakem

1 Atıf (Scopus)

Özet

Copper and zinc results of 98 rock samples, obtained by the colorimetric method were analysed statistically. Linear, quadratic and cubic trend surface analysis were applied to both original copper and zinc values and also to the copper/zinc ratios. Only quadratic trend surfaces were calculated for residual copper and zinc values. Goodness of fit method was also applied to the results obtained by trend surface analysis. -from Authors

Orijinal dilİngilizce
Sayfa (başlangıç-bitiş)551-567
Sayfa sayısı17
DergiBulletin - Technical University of Istanbul
Hacim44
Basın numarası3-4
Yayın durumuYayınlandı - 1991