Thermal behavior and kinetics of glass transition in B 2O 3 containing tungsten-tellurite glasses

M. Çelikbilek*, A. E. Ersundu, D. Yardimci, N. Solak, S. Aydin

*Bu çalışma için yazışmadan sorumlu yazar

Araştırma sonucu: ???type-name???Konferans katkısıbilirkişi

Özet

Thermal behavior and kinetics of glass transition in B 2O 3 containing tungsten-tellurite glasses was studied by using differential scanning calorimetry (DSC) and X-ray diffraction (XRD) techniques. Different compositions of the 0.80TeO 2 - (0.20-x)WO 3 - xB 2O 3 system (0 ≤ x ≤ 0.20 in molar ratio) were prepared with conventional melt-quenching technique at 750°C and it was aimed to investigate the effect of B 2O 3 addition on the vitrification behavior of tungsten-tellurite glasses. The kinetics of glass transition was studied under non-isothermal conditions and the glass transition activation energy, E g, was determined by modified Kissinger equation.

Orijinal dilİngilizce
Ana bilgisayar yayını başlığıMaterials Science and Technology Conference and Exhibition 2011, MS and T'11
Sayfalar55-61
Sayfa sayısı7
Yayın durumuYayınlandı - 2011
EtkinlikMaterials Science and Technology Conference and Exhibition 2011, MS and T'11 - Columbus, OH, United States
Süre: 16 Eki 201120 Eki 2011

Yayın serisi

AdıMaterials Science and Technology Conference and Exhibition 2011, MS and T'11
Hacim1

???event.eventtypes.event.conference???

???event.eventtypes.event.conference???Materials Science and Technology Conference and Exhibition 2011, MS and T'11
Ülke/BölgeUnited States
ŞehirColumbus, OH
Periyot16/10/1120/10/11

Parmak izi

Thermal behavior and kinetics of glass transition in B 2O 3 containing tungsten-tellurite glasses' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap