Özet
In this study, the effect of thermal oxidation on the dry sliding wear resistance of a Ti-6Al-4V alloy has been examined. Oxidation has introduced hard surface layers composed of TiO2 and oxygen diffusion zone beneath it. Hardness survey conducted under a load of 10 g with a Vickers pyramid indenter revealed that surface hardness increased from 450 to 1300 HV0,01 upon oxidation at 600 °C for 60 h, which was accompanied by significant improvement in wear resistance. Thus, the dry sliding wear rate of thermally oxidised Ti-6Al-4V alloy was almost negligible when compared to the as-received condition.
| Orijinal dil | İngilizce |
|---|---|
| Sayfa (başlangıç-bitiş) | 164-170 |
| Sayfa sayısı | 7 |
| Dergi | Surface and Coatings Technology |
| Hacim | 192 |
| Basın numarası | 2-3 |
| DOI'lar | |
| Yayın durumu | Yayınlandı - 21 Mar 2005 |
Parmak izi
Surface modification of a Ti-6Al-4V alloy by thermal oxidation' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.Alıntı Yap
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver