Özet
This paper investigates extraction of nickel and iron from a lateritic nickel ore from the Caldag region of Manisa in Turkey. The ore sample contains 1.2% Ni, 24.77% Fe and 0.062% Co. The process applied includes digestion with 40 wt-% sulfuric acid at 200 °C for 60 min, roasting at 700 °C for 15 min, leaching with water for 30 min at 1:5 solid/liquid ratio (by weight) and precipitation of the remaining iron at pH 3 and 60 °C. In order to improve nickel and cobalt extractions using the digestion-roasting- leaching-precipitation process (DRLP), Na2SO4 addition in the roasting stage was examined. Under the optimum conditions and in the presence of Na2SO4, 86.2% Ni and 94.2% Co extractions were obtained with almost zero iron content. As a result, 2.07 g dm-3 Ni, 0.12 g dm-3b c Co and 0.05 g dm-3 Fe could be achieved in the pregnant leach solution within nearly 2.5 hours.
| Orijinal dil | İngilizce |
|---|---|
| Sayfa (başlangıç-bitiş) | 564-574 |
| Sayfa sayısı | 11 |
| Dergi | Physicochemical Problems of Mineral Processing |
| Hacim | 52 |
| Basın numarası | 2 |
| DOI'lar | |
| Yayın durumu | Yayınlandı - 2016 |
Parmak izi
Separation of nickel and iron from lateritic ore using a digestion - roasting - leaching - precipitation process' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.Alıntı Yap
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver