Phase interaction in hydroxylapatite/lapo 4 composite

Celaletdln Ergun*, John W. Halloran, Chang Jun Bae, Filiz Çinar Şahin

*Bu çalışma için yazışmadan sorumlu yazar

Araştırma sonucu: Kitap/Rapor/Konferans Bildirisinde BölümKonferans katkısıbilirkişi

Özet

Hydroxylapatite composites with lanthanum phosphate were prepared with pressureless air sintering for hours at different temperatures between 500°C and 1300°C. The interaction between the phases was monitored with XRD analysis. At sintering temperatures higher than 700°C, hydroxylapatite and lanthanum phosphate phase reacted and formed Ca 8 La 2 (PO 4) 6O 2 as byproduct. In the mean time, hydroxylapatite decomposed and formed tricalcium phosphate.

Orijinal dilİngilizce
Ana bilgisayar yayını başlığıProceedings of 8th Biennial ASME Conference on Engineering Systems Design and Analysis, ESDA 2006
Yayın durumuYayınlandı - 2006
Etkinlik8th Biennial ASME Conference on Engineering Systems Design and Analysis, ESDA2006 - Torino, Italy
Süre: 4 Tem 20067 Tem 2006

Yayın serisi

AdıProceedings of 8th Biennial ASME Conference on Engineering Systems Design and Analysis, ESDA2006
Hacim2006

???event.eventtypes.event.conference???

???event.eventtypes.event.conference???8th Biennial ASME Conference on Engineering Systems Design and Analysis, ESDA2006
Ülke/BölgeItaly
ŞehirTorino
Periyot4/07/067/07/06

Parmak izi

Phase interaction in hydroxylapatite/lapo 4 composite' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap