Itaconic acid (methylene succinic acid)-acrylamide (IA-AAm) copolymers were synthesized with solution polymerization by using potassium persulphate. The potentiometric titration method was used to determine the copolymer compositions. The results were evaluated by various methods. The monomer reactivity ratios were found to be rIA = 0.99±0.04, rAAm = 0.58±0.02 with the Fineman-Ross, rIA = 1.05±0.10, rAAm = 0.62±0.06 with the Kelen-Tudos, and rIA = 1.36±0.11, rAAm = 0.77±0.06 with the Tidwell-Mortimer methods. As expected, IA is found to be the more reactive monomer in IA-AAm copolymers.
| Orijinal dil | İngilizce |
|---|---|
| Sayfa (başlangıç-bitiş) | 2651-2654 |
| Sayfa sayısı | 4 |
| Dergi | European Polymer Journal |
| Hacim | 36 |
| Basın numarası | 12 |
| DOI'lar | |
| Yayın durumu | Yayınlandı - Ara 2000 |
Parmak izi
Monomer reactivity ratios of itaconic acid and acrylamide copolymers determined by using potentiometric titration method' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.Alıntı Yap
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver