Özet

Membrane-based separation processes are part of most water purification plants worldwide. Industrial separation applications, primarily water purification and gas separation, can be improved with novel membranes or modification to existing ones. Atomic layer deposition (ALD) is an emerging technique that is proposed to upgrade certain kinds of membranes independent of their chemistry and morphology. ALD deposits thin, defect-free, angstrom-scale, and uniform coating layers on a substrate’s surface by reacting with gaseous precursors. The surface-modifying effects of ALD are described in the present review, followed by a description of various types of inorganic and organic barrier films and how these can be used in combination with ALD. The role of . ALD in membrane fabrication and modification is categorized into different membrane-based groups according to the treated medium, i.e., water or gas. In all membrane types, the ALD-based direct deposition of inorganic materials, mainly metal oxides, on the membrane surface can improve antifouling, selectivity, permeability, and hydrophilicity. Therefore, the ALD technique can broaden the applications of membranes to the treatment of emerging contaminants in water and air. Finally, the advancement, limitations, and challenges of ALD-based membrane fabrication and modification are compared to provide a comprehensive guideline for developing next-generation membranes with improved filtration and separation performance.

Orijinal dilİngilizce
Sayfa (başlangıç-bitiş)13825-13843
Sayfa sayısı19
DergiACS applied materials & interfaces
Hacim15
Basın numarası11
DOI'lar
Yayın durumuYayınlandı - 2023

Bibliyografik not

Publisher Copyright:
© 2023 American Chemical Society.

BM SKH

Bu sonuç, aşağıdaki Sürdürülebilir Kalkınma Hedefine/Hedeflerine katkıda bulunur

  1. SKH 6 - Temiz Su ve Sanitasyon
    SKH 6 Temiz Su ve Sanitasyon

Parmak izi

Membrane Fabrication and Modification by Atomic Layer Deposition: Processes and Applications in Water Treatment and Gas Separation' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap