Two types of Y-α-SiAlON composition, with different amounts of additional liquid phase were densified in a gas pressure sintering furnace using three different sintering cycles. One series of samples was heated up to 1825°C for 3 hrs, another group of samples was held at a lower temperature (1500°C or 1600°C) for 1 hr and then heated up to 1825°C for 3 hrs. The effect of the amounts of sintering additive and processing conditions on density and microstructure were evaluated.
| Orijinal dil | İngilizce |
|---|---|
| Sayfa (başlangıç-bitiş) | 1009-1012 |
| Sayfa sayısı | 4 |
| Dergi | Key Engineering Materials |
| Hacim | 206-213 |
| Basın numarası | II |
| Yayın durumu | Yayınlandı - 2001 |
| Harici olarak yayınlandı | Evet |
| Etkinlik | 7th Conference and Exhibition of the European Ceramic Society - Brugge, Belgium Süre: 9 Eyl 2001 → 13 Eyl 2001 |
Parmak izi
Improvement of elongated α-SiAlON ceramics by variation of the processing conditions and amounts of additives' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.Alıntı Yap
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver