Impact-sliding wear failures mostly occur in complex tribological contact systems such as working parts of combustion engines, metal-forming dies, etc. The impact-sliding test method allows for examining both the effect of cyclic impact and sliding contacts. In this study, the impact-sliding wear test was conducted on Stellite 6 and Stellite 12 hardfacings produced by using Tungsten Inert Gas welding was investigated at room and high temperatures. Microstructural examinations and impact-sliding wear tests revealed that even though examined hardfacings exhibited almost similar microstructural features, the impact-sliding wear loss of the Stellite 12 hardfacing was relatively higher when compared to Stellite 6 hardfacing both at room temperature and 600 °C.

Orijinal dilİngilizce
Makale numarası128762
DergiMaterials Chemistry and Physics
Hacim313
DOI'lar
Yayın durumuYayınlandı - 1 Şub 2024

Bibliyografik not

Publisher Copyright:
© 2023 Elsevier B.V.

Finansman

We would like to express our sincere gratitude to Prof. Dr. Hüseyin Çimenoğlu and Res. Assist. Mertcan Kaba from Metallurgical and Materials Engineering Department of Istanbul Technical University. The impact-sliding test equipment used in this study has been funded by TUBITAK TEYDEB with grant number 5160013. Also, we would like to thank MSc. Seçkin Özkurt from Süpsan Automotive Parts Ind. Trade. Inc. We would like to express our sincere gratitude to Prof. Dr. Hüseyin Çimenoğlu and Res. Assist. Mertcan Kaba from Metallurgical and Materials Engineering Department of Istanbul Technical University. The impact-sliding test equipment used in this study has been funded by TUBITAK TEYDEB with grant number 5160013 . Also, we would like to thank MSc. Seçkin Özkurt from Süpsan Automotive Parts Ind. Trade. Inc.

FinansörlerFinansör numarası
TUBITAK TEYDEB5160013
Istanbul Teknik Üniversitesi

    Parmak izi

    Impact sliding wear behavior of Stellite 6 and Stellite 12 hardfacings' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

    Alıntı Yap