̇Iki deǧerli demir sülfattan demir tozu üretimi

E. Açma*, M. Ş Sönmez

*Bu çalışma için yazışmadan sorumlu yazar

Araştırma sonucu: ???type-name???Makalebilirkişi

Özet

The production of iron powder from concentrated iron solutions obtained during surface finishing (pickling) carried out to produce zinc or tin coated thin sheets, was investigated. Goethite precipitation from the waste pickle liquors-dehydration-reduction method was used to produce iron powder. In the experiments, the optimum parameters of the chosen method were investigated. The iron powders produced had an average grain size of 4-5 μm, and a specific surface area of 1.2 m2/g, and the product consisted of 99.75% Fe, 0.03% C, 0.015% P and 0.01% S.

Tercüme edilen katkı başlığıProduction of iron powder from iron (II) sulphate
Orijinal dilTürkçe
Sayfa (başlangıç-bitiş)211-218
Sayfa sayısı8
DergiTurkish Journal of Engineering and Environmental Sciences
Hacim25
Basın numarası3
Yayın durumuYayınlandı - 2001

Keywords

  • Dehydration
  • Goethite
  • Iron powder
  • Reduction

Parmak izi