Aladaǧ (Kayseri-Turkey) lead-zinc sulfide-oxide ores contain 10.17% Pb, 10.98 %Zn, 164 g/t Cd and 57 g/t Ag. During the laboratory scale flotation tests of these ores, it was found that almost all zinc was remained in the tailings that contain 12.31% Zn, 1.35%Pb, 198.3 g/t Cd, and 22.3%Fe. Three different methods were studied such as basic (NaOH) leaching, roasting+acidic (H2SO4) leaching and direct acidic (H2SO 4) leaching for recovering metals that these tailings contain. In the direct acidic leaching, which gave the best results, dissolution efficiencies of 91.5% zinc, 78.2% cadmium, and 14.3% iron were reached at the optimum leaching conditions while Pb remained in the leach residues and the acid consumption was 422.3 kg/ton of tailings.

Orijinal dilİngilizce
Ana bilgisayar yayını başlığıSohn International Symposium
Ana bilgisayar yayını alt yazısıAdvanced Processing of Metals and Materials - Proceedings of the International Symposium
Sayfalar387-395
Sayfa sayısı9
Yayın durumuYayınlandı - 2006
Etkinlik2006 TMS Fall Extraction and Processing Division: Sohn International Symposium - San Diego, CA, United States
Süre: 27 Ağu 200631 Ağu 2006

Yayın serisi

Adı2006 TMS Fall Extraction and Processing Division: Sohn International Symposium
Hacim3

???event.eventtypes.event.conference???

???event.eventtypes.event.conference???2006 TMS Fall Extraction and Processing Division: Sohn International Symposium
Ülke/BölgeUnited States
ŞehirSan Diego, CA
Periyot27/08/0631/08/06

Parmak izi

Evaluation of lead-zinc flotation tailings' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap