Electrospinning Combined with Atomic Layer Deposition to Generate Applied Nanomaterials: A Review

  • Sesha Vempati*
  • , Kugalur Shanmugam Ranjith
  • , Fuat Topuz
  • , Necmi Biyikli
  • , Tamer Uyar*
  • *Bu çalışma için yazışmadan sorumlu yazar
  • Indian Institute of Technology Bhilai
  • Dongguk University
  • Bilkent University
  • University of Connecticut
  • Cornell University

Araştırma çıktısı: Dergi yayınıİnceleme makalesiHakem

38 Atıf (Scopus)

Özet

Combining different material processing techniques is one of the keys to obtain materials that depict synergistic properties. In this review, we have reviewed a combination of two highly potential techniques, namely, electrospinning and atomic layer deposition (ALD), in the view of various applications. Over the past 10 years, our research groups are involved in the exploration of employing this combination for a range of applications. We also include some basic information on both the processes and diversity of nanostructures as a result of their combination. Nonwoven nanofiber membranes are excellent candidates for a wide range of applications. Also, they can act as templates to produce various other kinds of nanostructures when combined with ALD in small/large scale production. These nanostructures could be used as such or further subjected to other processing techniques yielding hierarchical structures. In this review, we exclusively survey and highlight the unique capabilities of combined electrospinning and ALD for applications in catalysis, photocatalysis, solar cells, batteries and gas sensors.

Orijinal dilİngilizce
Sayfa (başlangıç-bitiş)6186-6209
Sayfa sayısı24
DergiACS Applied Nano Materials
Hacim3
Basın numarası7
DOI'lar
Yayın durumuYayınlandı - 24 Tem 2020
Harici olarak yayınlandıEvet

Bibliyografik not

Publisher Copyright:
Copyright © 2020 American Chemical Society.

BM SKH

Bu sonuç, aşağıdaki Sürdürülebilir Kalkınma Hedefine/Hedeflerine katkıda bulunur

  1. SKH 7 - Erişilebilir ve Temiz Enerji
    SKH 7 Erişilebilir ve Temiz Enerji

Parmak izi

Electrospinning Combined with Atomic Layer Deposition to Generate Applied Nanomaterials: A Review' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap