Contribution of galvanic coupling with TiN, TiAlN, and CrN to the corrosion of steel in neutral and acidic chloride solutions

Burçak Avcı, Kürşat Kazmanlı, Burak Evren, Mustafa Ürgen*

*Bu çalışma için yazışmadan sorumlu yazar

Araştırma sonucu: Dergiye katkıMakalebilirkişi

4 Atıf (Scopus)

Özet

The inherent defective morphology of the physical vapor deposition (PVD) hard coatings limits their corrosion protective ability. We examined the impact of nitride-based PVD coatings, including TiN, TiAlN, and CrN deposited on inert substrates by cathodic arc PVD method (CA-PVD), on the galvanic corrosion of carbon steel. Their contribution was evaluated by zero-resistance ammeter (ZRA) and electrochemical impedance spectroscopy (EIS) in 3.5 wt.% NaCl at pH 2 and 6, with and without aeration. The results indicated the prominent role of the coating type and the coupling environment on the generated galvanic currents. Immersion tests for the TiN-, TiAlN-, and CrN-coated steel cross-sections visually verified these results. The galvanic current contribution was distinct in environments where oxygen reduction is the dominant cathodic reaction. However, the layers' contribution to galvanic corrosion was minimal in deaerated acidic solutions, which is attributed to the high bonding strength of adsorbed intermediates to the coating surfaces.

Orijinal dilİngilizce
Sayfa (başlangıç-bitiş)1390-1399
Sayfa sayısı10
DergiMaterials and Corrosion
Hacim74
Basın numarası9
DOI'lar
Yayın durumuYayınlandı - Eyl 2023

Bibliyografik not

Publisher Copyright:
© 2023 Wiley-VCH GmbH.

Finansman

The authors wish to thank Prof. Dr. Servet Timur for valuable discussions on reduction kinetics. The help of Dr. Doga Bilican and Dr. Nuri Solak is appreciated for the SEM image used in the graphical abstract.

Parmak izi

Contribution of galvanic coupling with TiN, TiAlN, and CrN to the corrosion of steel in neutral and acidic chloride solutions' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap