Boron minerals are generally concentrated using attrition methods followed by screening and classification to remove clay minerals in industrial scale. Physical concentration methods are used in Kestelek Boron Mine for the concentration of colemanite. Because of the inefficient process operation, the tailings containing about 20% B2O3 are discarded into the tailings pond. In this study, colemanite tailings sample taken from tailings pond was treated using scrubbing + screening followed by flotation to recover the lost boron. As a result of the experimental studies, a concentrate containing 44.5% B2O3 was produced with 68.4% B 2O3 recovery.

Orijinal dilİngilizce
Sayfa (başlangıç-bitiş)368-369
Sayfa sayısı2
DergiMinerals Engineering
Hacim19
Basın numarası4
DOI'lar
Yayın durumuYayınlandı - Nis 2006

Parmak izi

Beneficiation of colemanite tailings by attrition and flotation' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap