Özet
The tailings produced from the calcination of Bigadic colemanite ore are upgraded by means of a gravity concentration method. The experiments were conducted in two separate fractions. The coarse (-1+0.5 mm) and the fine (-0.5 mm) tailing fractions containing respectively 20.01% and 36.31% B2O3 were treated on a Deister Superduty Diagonal Deck laboratory concentrating table. Under the optimum conditions, a colemanite concentrate assaying 51.01% B2O3 with 68.67% recovery was obtained. The combined results of calcination and tabling resulted in a final concentrate containing 51.88% B2O3 with an 84.41% recovery rate.
| Orijinal dil | İngilizce |
|---|---|
| Sayfa (başlangıç-bitiş) | 215-217 |
| Sayfa sayısı | 3 |
| Dergi | Powder Technology |
| Hacim | 77 |
| Basın numarası | 2 |
| DOI'lar | |
| Yayın durumu | Yayınlandı - Kas 1993 |
Parmak izi
Beneficiation of calcined colemanite tailings' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.Alıntı Yap
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver