An investigation of copper and selenium recovery from copper anode slimes

Yasin Kilic*, Guldem Kartal, Servet Timur

*Bu çalışma için yazışmadan sorumlu yazar

Araştırma sonucu: Dergiye katkıMakalebilirkişi

91 Atıf (Scopus)

Özet

In this study, an alternative method was investigated for the recovery of copper and selenium from copper anode slimes, supplied from Sarkuysan Co. in Turkey. The proposed process was composed of two hydrometallurgical steps; decopperization in H2SO4 medium and dissolution of selenium into NaOH solution. The effects of oxygen flow rate and solution temperature on the decopperization of anode slimes were examined in H 2SO4 medium and copper recovery was achieved with an efficiency of 94%. The X-ray diffraction (XRD) analysis revealed Cu 2Se as a remaining phase of copper in anode slimes after the decopperization process. Following the decopperization stage, anode slimes were treated with NaOH solution in order to dissolve selenium. The influences of NaOH concentration, temperature and various types of oxidants on selenium dissolution were inspected. The uniqueness of this technique is that it provides to have an efficiency of selenium recovery as high as 86.8% in an alkaline solution (4 M NaOH) under atmospheric conditions without requiring an autoclave.

Orijinal dilİngilizce
Sayfa (başlangıç-bitiş)75-82
Sayfa sayısı8
DergiInternational Journal of Mineral Processing
Hacim124
DOI'lar
Yayın durumuYayınlandı - 2013

Parmak izi

An investigation of copper and selenium recovery from copper anode slimes' araştırma başlıklarına git. Birlikte benzersiz bir parmak izi oluştururlar.

Alıntı Yap