TY - JOUR
T1 - Acidic leaching of scheelite concentrate and production of hetero-poly-tungstate salt
AU - Gürmen, Sebahattin
AU - Timur, Servet
AU - Arslan, Cüneyt
AU - Duman, Ismail
PY - 1999
Y1 - 1999
N2 - The aim of this study is to investigate the utility of adding chelating agent during hydrochloric acid leaching of low-grade scheelite concentrates, obtained from Uludag, Bursa (Türkiye). Examined parameters were as follows; leaching conditions, selective precipitation of tungsten salt from the acidic leach solution in which tungsten exists as hetero-poly-tungstate, the optimum precipitation conditions, the possibility of obtaining pure and nano-sized tungsten salt. Chelating agent leaching of scheelite concentrates in acidic solutions involves fewer process steps as compared to the classical methods. Furthermore, this route enables production of pure WO3 under prevalent conditions and without generating any spent liquor. The optimum leaching conditions were found to be 80°C, 2 M HCl, 1/10 solid/liquid ratio, stirring speed of 900 min-1 and W/PO43- weight ratio of 7/1. A tungsten leaching efficiency of 98% was reached under these conditions. It was also possible to selectively precipitate a pure (over 99%) tungstate salt, within minutes, from the poly-tungstate solution at 25°C by adding a 'chelate breaking agent' at a NH4+/WO3 weight ratio of ≥ 1/4.
AB - The aim of this study is to investigate the utility of adding chelating agent during hydrochloric acid leaching of low-grade scheelite concentrates, obtained from Uludag, Bursa (Türkiye). Examined parameters were as follows; leaching conditions, selective precipitation of tungsten salt from the acidic leach solution in which tungsten exists as hetero-poly-tungstate, the optimum precipitation conditions, the possibility of obtaining pure and nano-sized tungsten salt. Chelating agent leaching of scheelite concentrates in acidic solutions involves fewer process steps as compared to the classical methods. Furthermore, this route enables production of pure WO3 under prevalent conditions and without generating any spent liquor. The optimum leaching conditions were found to be 80°C, 2 M HCl, 1/10 solid/liquid ratio, stirring speed of 900 min-1 and W/PO43- weight ratio of 7/1. A tungsten leaching efficiency of 98% was reached under these conditions. It was also possible to selectively precipitate a pure (over 99%) tungstate salt, within minutes, from the poly-tungstate solution at 25°C by adding a 'chelate breaking agent' at a NH4+/WO3 weight ratio of ≥ 1/4.
KW - Hetero-poly-tungstate salt
KW - Leaching
KW - Scheelite concentrates
UR - http://www.scopus.com/inward/record.url?scp=0033075113&partnerID=8YFLogxK
U2 - 10.1016/s0304-386x(98)00080-2
DO - 10.1016/s0304-386x(98)00080-2
M3 - Article
AN - SCOPUS:0033075113
SN - 0304-386X
VL - 51
SP - 227
EP - 238
JO - Hydrometallurgy
JF - Hydrometallurgy
IS - 2
ER -