Shear bond strength of resin luting cement to glass-infiltrated porous aluminum oxide cores

Deniz Sen*, Erdal Poyrazoglu, Betül Tuncelli, Gültekin Göller

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

48 Citations (Scopus)

Abstract

Statement of problem. Resin bonding surface treatment methods for conventional silica-based dental ceramics are not reliable for glass infiltrated high alumina content In-Ceram ceramics. Purpose. This study developed an alternative surface treatment to improve resin bonding of glass-infiltrated aluminum oxide ceramic blasting with diamond particles and then observed the efficiency of this treatment. Material and methods. In-Ceram test specimens were prepared and divided into 2 groups. All specimens were sandblasted with Al2O3, and blasted with diamond particles and 2 adhesive resins were applied. After bonding and storage in humid conditions, shear bond strength values were measured with a universal testing machine. Surface roughness and fracture interfaces were determined with a perthometer and a SEM. Results. The highest bond strength was obtained on the samples blasted with diamond particles (group 11). The differences between the 2 groups and the 2 adhesive resin cements were both statistically significant. Conclusion. Panavia-Ex cement exhibited higher bond strength than Super-Bond cement. This higher bond strength was attributed to ceramic oxide and ester bond and the mechanical properties of Panavia-Ex cement.

Original languageEnglish
Pages (from-to)210-215
Number of pages6
JournalJournal of Prosthetic Dentistry
Volume83
Issue number2
DOIs
Publication statusPublished - Feb 2000