Abstract
Acrylamide was polymerized by eeric ion Ce (IV)-4,4′-azobis(4-cyano pentanol)(ACP) redox pair in aqueous nitric acid under nitrogen atmosphere. The rate of polymerization is proportional to [M] 2 ,[ACP] and [Ce(IV)] -1 . Termination mechanism which was exclusively linear offered one azo group per polymeric chain. The obtained polyacrylamide can be used as a water soluble initiator for vinyl polymerization.
| Original language | English |
|---|---|
| Pages (from-to) | 483-488 |
| Number of pages | 6 |
| Journal | Polymer Bulletin |
| Volume | 22 |
| Issue number | 5-6 |
| DOIs | |
| Publication status | Published - Dec 1989 |
Fingerprint
Dive into the research topics of 'Polymerization of acrylamide initiated by the redox system Ce(IV)-4,4′-azobis (4-cyano pentanol)'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver