Abstract
Two types of Y-α-SiAlON composition, with different amounts of additional liquid phase were densified in a gas pressure sintering furnace using three different sintering cycles. One series of samples was heated up to 1825°C for 3 hrs, another group of samples was held at a lower temperature (1500°C or 1600°C) for 1 hr and then heated up to 1825°C for 3 hrs. The effect of the amounts of sintering additive and processing conditions on density and microstructure were evaluated.
| Original language | English |
|---|---|
| Pages (from-to) | 1009-1012 |
| Number of pages | 4 |
| Journal | Key Engineering Materials |
| Volume | 206-213 |
| Issue number | II |
| Publication status | Published - 2001 |
| Externally published | Yes |
| Event | 7th Conference and Exhibition of the European Ceramic Society - Brugge, Belgium Duration: 9 Sept 2001 → 13 Sept 2001 |
Keywords
- Additive Content
- Grain Morphology
- Process Conditions
- α-SiAlON
Fingerprint
Dive into the research topics of 'Improvement of elongated α-SiAlON ceramics by variation of the processing conditions and amounts of additives'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver