Abstract
W-1 wt% Ni (W1Ni) matrix composites reinforced with TiB2 and La2O3 particles were fabricated via mechanical alloying and activated sintering methods. Powder blends with compositions of W1Ni2 wt% TiB2x wt% La2O3 (x = 0:5, 1) were mechanically alloyed for 6 and 12 h. The results showed that increase in mechanical alloying duration to 12 h causes the decline of grain sizes of the W-Ni matrix to nanoscales. TiB2/La2O3 particles have a significant effect on the density/microhardness values and wear amounts of the sintered samples.
| Original language | English |
|---|---|
| Pages (from-to) | 309-311 |
| Number of pages | 3 |
| Journal | Acta Physica Polonica A |
| Volume | 123 |
| Issue number | 2 |
| DOIs | |